Cracks

Cracks in walls in Adelaide: when to worry

Most cracks in Adelaide homes are cosmetic, but some point to footing movement on reactive clay. How to read width, pattern and growth, with the engineer's crack scale and the local figures.

Diagonal crack running through bluestone blocks and lime mortar beside red-brick quoins and a timber window frame

In short

Most cracks in walls are cosmetic: hairline cracks under 1 mm that only need filling. Worry when a crack reaches 5 mm, keeps growing, steps through brickwork or comes with sticking doors and sloping floors. Much of Adelaide sits on highly reactive clay, and ABS data for 2019–20 show 6.5% of South Australian houses have major cracks in ceilings or floors, the highest share of any state or territory.

Key takeaways

  • Under 1 mm is usually cosmetic. From 5 mm, AS 2870 rates the damage as moderate.
  • Growth beats width: a crack that is still opening matters more than a wide one that stopped years ago.
  • On reactive clay, cracks often open over a dry summer and close in a wet winter. Readings through the seasons show which kind you have.
  • Diagnose first, then price a repair. The cause is often a leak, a downpipe or a tree, not a failed footing.
  • Crumbling mortar and white salts low on an old wall are usually salt damp, not movement.

A crack is often the first thing that sends an Adelaide homeowner to a structural engineer. It is a symptom, not a diagnosis. Before anyone fills it, pins it or underpins the wall, you want three answers: how wide it is, whether it is still moving and what is moving the house. This guide covers cracks in brick, brick veneer, bluestone and plaster, and what Adelaide's ground has to do with them.

Cracks in walls: quick facts

Usually cosmetic
Hairline cracks under 1 mm that have stopped moving
Get it checked
5 mm or wider, growing, stepped or tapered
Adelaide ground
Much of it highly reactive clay; every site differs
How common
6.5% of SA houses have major ceiling or floor cracks (ABS, 2019–20)
How to watch
Repeat readings through the dry and wet months
Our crack report
From $990 + GST ($1,089 inc GST)

How do you tell if a crack in a wall is serious?

Judge a crack on four things together: its width, whether it is growing, its shape, and what the rest of the house is doing. Any one of them alone can mislead.

How wide

Read the widest point. Below 1 mm is normally a finishing issue; at 5 mm and above AS 2870 calls the damage moderate.

Still moving?

A crack that passes your pencil marks over a few months is telling you the cause is still at work.

What shape

Steps, diagonals from corners, tapers and horizontal runs each point to a different kind of movement.

The rest of the house

Doors that bind, floors that slope and cornices pulling away mean more than one wall has moved.

Engineers grade wall cracks with the damage categories in AS 2870-2011, the Australian Standard for residential slabs and footings. It is the nearest thing Australia has to an official crack chart, and our reports use it.

  1. Cat 0Negligible< 0.1 mm

    Hairline cracks.

  2. Cat 1Very slight< 1 mm

    Fine cracks which do not need repair.

  3. Cat 2Slight< 5 mm

    Cracks noticeable but easily filled. Doors and windows stick slightly.

  4. Cat 3Moderate5–15 mm

    Cracks can be repaired; some wall may need replacing. Doors and windows stick, service pipes can fracture, weathertightness often impaired.

  5. Cat 4Severe15–25 mm

    Extensive repair: sections of wall broken out and replaced. Frames distort, walls lean or bulge, some loss of bearing in beams.

  6. Cat 5Very severe> 25 mm

    Major repair, partial or complete rebuilding. Beams lose bearing, walls lean badly and need shoring. Danger of instability.

Figure 1Damage categories for walls, with approximate crack widths. Crack width is a guide only: the number, pattern and location of cracks also matter.Source: AS 2870-2011 Residential slabs and footings, Appendix C, Table C1.

The scale is a starting point

A wall with many fine cracks can be in worse shape than one with a single wide crack, and an active crack outranks a stable one. Engineers read the category alongside the pattern and a series of readings.

What do different crack patterns mean?

A crack's shape shows the direction of movement. These four patterns are the ones an engineer reads first.

Four crack patterns an engineer reads first

Four common crack patterns in brick walls Four brick wall panels. Panel A shows a stepped crack climbing diagonally through the mortar joints. Panel B shows a diagonal crack running from the top corner of a window. Panel C shows a vertical crack that is wider at the top than the bottom. Panel D shows a horizontal crack running along a mortar course. A · Stepped crack B · From a window corner wider narrower C · Vertical, tapered D · Horizontal crack
  • A · Stepped: follows the mortar joints up and across. Often a sign one part of the wall has moved relative to another.
  • B · From a window or door corner: openings concentrate stress, so movement tends to show at their corners first.
  • C · Vertical: note whether it's wider at the top or the bottom. The taper shows which way the wall has moved.
  • D · Horizontal: can point to sideways pressure, roof thrust or corroding wall ties. Worth an engineer's look.
Figure 2The pattern, width, length and location of a crack matter more than any single measurement. These are common readings, not a diagnosis: the cause is confirmed on site.Illustrative diagram. Prepared by Adelaide Structures.

What do cracks in brick, brick veneer and bluestone walls mean?

In masonry a crack takes the easiest route, usually through the mortar, so a crack stepping diagonally through the joints is the classic sign that part of the wall has dropped or lifted relative to the rest. A crack that cuts straight through bricks or stones points to larger or quicker movement.

1960s cream brick house with a tiled roof and a stair-step crack running down from the corner of the front window
Figure 3A stair-step crack from the corner of a window in a 1960s brick house. Openings are the weak points in a wall, so footing movement often shows there first.
  • A staircase through the joints often traces back to a footing moving, for example where clay has dried out under one corner.
  • A vertical crack that narrows at one end: measure the top and the bottom, because the wide end shows the direction of movement.
  • A horizontal crack along one mortar course can come from soil or water pushing sideways, a roof spreading the wall, or rusting wall ties.
  • The same crack inside and out means the wall itself has moved, not just the plaster or render on it.

Adelaide's bluestone and sandstone villas are laid in soft lime mortar, which lets an old wall move a little and crack along its joints instead of through the stone. Many carry cracks that were repointed decades ago and haven't moved since. A crack with a clean, fresh face, or one splitting newer cement repointing, is the one to watch. Our bluestone homes guide covers these walls in detail.

Why do houses in Adelaide crack?

Most cracking in Adelaide houses comes from water and clay: reactive clay drying or wetting under the footings, often helped along by trees, leaking pipes or poor drainage. InDaily's 2022 report noted that Adelaide houses are mostly "solid masonry on dwarf wall footing systems or raft slabs", and heavy masonry shows ground movement quickly.

How common house faults are in South Australia

  • South Australiastructural problems of any kind12.2%
  • Australiastructural problems of any kind11.0%
  • South Australiamajor cracks in ceilings or floors6.5%
Figure 4Share of houses, 2019–20. South Australia's share with major ceiling or floor cracks was the highest of any state or territory.Source: ABS data for 2019–20, reported by InDaily (3 August 2022).

The ground explains much of it. A state soil study of the Adelaide area, by Mines and Energy SA and CSIRO, found that "deeper clays are equally reactive and are responsible for many building cracks and footing failures", and linked footing problems to "substrate defects, gilgai, trees, changes to site environment, and seismicity". A 2016 study of one north-eastern site found the clay reacted to ponding water and leaking service pipes. Adelaide University's 2026 research cites an earlier estimate that almost 480,000 South Australian houses built before 1981 had incurred $1.5 billion in shrinkage-crack damage.

What moves a house? Four common causes

Common causes of house movement Cross-section of a single-storey house on strip footings. A tree on the left has roots reaching under the left footing. A band of reactive clay runs under the house with shrinkage cracks. On the right, a leaking pipe wets the soil, and an area of loose fill sits under the right footing. Numbered red markers point to each cause. 1 2 3 4 Firmer ground
  1. Trees and roots draw moisture from the soil near a footing, so clay under that side shrinks.
  2. Reactive clay swells when wet and shrinks when dry, moving footings with the seasons.
  3. Leaking pipes or poor drainage soak and soften the ground under part of the house.
  4. Poorly compacted fill keeps settling under a footing long after the house is built.
Figure 5Simplified section, not to scale. Most movement has more than one contributor, which is why the cause should be confirmed before anyone prices a repair.Illustrative diagram. Prepared by Adelaide Structures.

Because water and trees start so much of it, the first fix is often a plumber, a gutter or an arborist, not a builder. Trees close to a house need care in SA: within the Regulated and Significant Tree Overlay, removing a regulated or significant tree, or substantially damaging its roots, needs approval. Read trees and house cracks in SA and our guide to Adelaide's reactive clay.

Is the crack seasonal or still getting worse?

A seasonal crack breathes with the weather, opening as the clay dries and closing as it wets, while a progressive crack ends each year wider than it started; only readings across dry and wet months tell them apart. On one Adelaide site, Adelaide University recorded cracks in the soil itself 5 to 40 mm wide and up to 1 m deep, at their worst in March and April. Seasonal movement can often be calmed with drainage and steady moisture. Progressive movement needs its cause found and, sometimes, a repair designed.

Cosmetic or structural: how do the signs compare?

A cosmetic crack is fine, stable and sits in the surface finish; a structural crack is wider, still moving or patterned, and goes through the wall.

CheckPoints to cosmeticPoints to structural: get advice
WidthHairline, under 1 mm5 mm or more, or clearly tapered
MovementUnchanged over yearsLengthening, widening, or cycling with the seasons
ShapeShort, random, along sheet jointsStaircase through brickwork, diagonal from openings, horizontal
DepthPaint, plaster or render onlyRight through the wall, visible on both faces
CompanyNothing else wrongBinding doors, sloping floors, gaps at cornices or skirtings
TimingAppeared once, then stoppedFollowed a leak, a dry summer, tree work or digging next door

A guide only. The cause is confirmed on site. Crumbling at the base of an old wall is a different problem: see salt damp or structural cracking.

How do you monitor a crack in a wall yourself?

Keep a dated record for a few months: a short series of readings tells an engineer far more than one photo, and it is the first step in proper crack monitoring.

  1. First visit

    Pencil the tips

    Rule a short line across each end of the crack and write the date beside it.

  2. First visit

    Read the width

    Read the widest point with a crack-width card or fine steel rule, and mark the spot.

  3. First visit

    Photograph with a scale

    Square-on, with a ruler beside the crack, from a spot you can return to.

  4. Monthly or so

    Repeat through the year

    Same spot, same method, plus a reading after a long dry spell or heavy rain.

  5. On any change

    Act on it

    Past the marks, wider, or joined by new cracks: the movement is active, so book an engineer.

When should you call a structural engineer about cracks?

Call a structural engineer when any of these signs shows up, or when you want an independent answer before spending money on a repair.

  • The crack reaches 5 mm, or is clearly wider at one end
  • It has passed your pencil marks, or new cracks keep joining it
  • Doors and windows have started binding, or cornices are pulling away
  • A floor has developed a slope, or floor tiles are cracking in a line
  • You've been quoted for underpinning or resin injection and want a second opinion
  • The house you're buying shows cracking the inspector couldn't explain

Get the diagnosis before the repair quote

Our cracks and footing movement report grades the cracks against AS 2870, finds the likely cause and lists your options, from $990 + GST ($1,089 inc GST). Already holding an underpinning quote? Our independent second opinion starts from $350 + GST ($385 inc GST).

Do

  • Date, measure and photograph the crack
  • Look for leaking taps, pipes, gutters and downpipes
  • Note when you first saw it and what the weather was doing
  • Get an engineer's view that isn't tied to a repair

Don't

  • Patch a wide crack before anyone has measured it
  • Treat underpinning as the default answer
  • Take advice only from the company selling the fix
  • Wait out a crack that keeps opening

Sources

  1. Standards Australia, AS 2870-2011 Residential slabs and footings. Appendix C, Table C1: classification of damage to walls
  2. InDaily, Cracking up: SA's nation-leading house faults (3 August 2022). ABS data for 2019–20; comments from Master Builders SA
  3. Sheard and Bowman (1996), soils of the Adelaide area, Mines and Energy SA and CSIRO (SARIG document RB9400009)
  4. Sheard and others (2016), reactive soil study, SARIG report d20011047
  5. Adelaide University, Stronger home foundations needed to withstand climate change (9 September 2026)
  6. CSIRO, Foundation Maintenance and Footing Performance: a homeowner's guide (formerly Building Technology File 18)

FAQ

Cracks in walls: FAQs

Still unsure? Call 08 7083 9853 or send photos for a fixed quote.

When should I worry about cracks in walls?

Worry when a crack reaches 5 mm, keeps getting longer or wider, steps through brickwork, tapers, or arrives with doors that stick and floors that slope. Any one of those is worth a structural engineer's visit.

Are stair-step cracks in brick walls serious?

They can be. A stair-step crack through the mortar joints usually means part of the wall has dropped or lifted relative to the rest, often from clay drying or wetting under one corner. Measure it and watch it; if it is 5 mm or more, or growing, have it assessed.

Why do so many Adelaide houses crack?

Much of Adelaide sits on highly reactive clay that swells when wet and shrinks as it dries, and most houses are solid masonry on dwarf wall footings or raft slabs. ABS data for 2019–20 show 6.5% of South Australian houses have major cracks in ceilings or floors, the highest share in Australia.

Why do cracks open in summer and close in winter?

The clay under the footings dries and shrinks over a hot summer, then swells as it wets again. Adelaide University recorded soil cracks up to 1 m deep on one Adelaide site, deepest in March and April.

Can I just fill the crack?

A fine crack that hasn't moved can be filled and painted. Leave a wide or active crack alone until it has been measured and the cause found, because filler hides the evidence and the crack usually comes back.

Do cracks mean my house needs underpinning?

Usually not on their own. Leaking pipes, poor drainage, downpipes and trees cause a lot of cracking, and fixing the cause, then watching the crack, is often enough. Get an independent diagnosis before anyone quotes for underpinning.

How much is a crack report in Adelaide?

Our cracks and footing movement report starts from $990 + GST ($1,089 inc GST), with a fixed quote in under 20 minutes on average, during business hours. It grades each crack on the AS 2870 scale, gives the likely cause and sets out the options.

Who should I call about cracks in my house?

An independent structural engineer, ideally one with no repair to sell. The engineer's job is to find the cause and say whether any repair is needed, before a contractor prices one.